Why ASA
- UV and weather resistance: keeps its colour and strength outdoors for years
- Heat resistance: slightly higher than ABS, up to about 100 °C
- Clean matte surface with no extra finishing
- Post-processing: sands, glues and paints just like ABS
Technical data (TDS)
| Property | Standard | Value |
|---|---|---|
| Heat deflection temperature (HDT), 0.45 MPa | ISO 75 | 100 °C |
| Heat deflection temperature (HDT), 1.8 MPa | ISO 75 | 92 °C |
| Vicat softening temperature | ISO 306 | 106 °C |
| Tensile strength along layers (X-Y) | ISO 527 | 37 MPa |
| Flexural modulus, stiffness (X-Y) | ISO 178 | 1920 MPa |
| Charpy impact strength, unnotched (X-Y) | ISO 179 | 41 kJ/m² |
Typical values from the filament maker’s technical data sheet (TDS), measured on standard test specimens. X-Y is along the layers, Z is between layers. The strength of a finished part also depends on its shape, print orientation, infill and wall thickness, so we choose these for the load. We will send the full TDS on request.
Where we use it
- Exterior car parts: mirror housings, grilles, trims, holders
- Outdoor enclosures for sensors, cameras and electronics
- Garden and boat equipment parts
- Signs, holders and mounts for facades and fences
When another material is a better fit
- Indoor parts: ABS, usually slightly cheaper
- When you need more stiffness: ASA-CF with carbon fibre
- When you need more strength and heat resistance: PC or PAHT-CF
FAQ
How long does an ASA part last outdoors?
ASA is made for outdoor use: it keeps its colour and mechanical properties under long exposure to sun, rain and frost, where ABS and PLA would start to fade and crack.
Is ASA suitable for exterior car parts?
Yes, it is one of the most popular materials for exterior car parts. Where loads are higher we recommend ASA-CF.
Price
We print ASA parts from €10 (VAT included). The price depends on size, quantity and requirements; we send an exact quote within one working day. → Get a quote